Charpy Impact, Notched 3.48 J/cm²
16.6 ft-lb/in²
Covestro Bayflex® 110-50 Polyurethane
Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.