Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.10 J/cm² | 38.5 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Charpy Impact, Notched | 8.10 J/cm² | 38.5 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® PSB 286 PA6, Conditioned Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |