Mechanical Properties Metric English Comments
Charpy Impact, Notched 12.8 J/cm²
60.9 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East)
GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi..
Charpy Impact, Notched 12.8 J/cm²
60.9 ft-lb/in²
ISO 179
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re..