Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® CS 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Charpy Impact, Notched | >= 13.0 J/cm² | >= 61.9 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene Applications which require a good combination between impact and wear resistance - technical and porous parts, filters, compression molded sheets.Information provided by Braskem. |
|||
Charpy Impact, Notched | >= 13.0 J/cm² | >= 61.9 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 4041 Ultra High Molecular Weight Polyethylene Applications which require a good combination between impact and wear resistance - use of pigments and/or additives - technical and porous parts, filters, compression molded sheets.Information provi.. |