Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.59 J/cm²
7.57 ft-lb/in²
Eastman Tenite 105-28 Cellulose Acetate  (discontinued **)
28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.59 J/cm²
7.57 ft-lb/in²
Eastman Tenite 105-33 Cellulose Acetate  (discontinued **)
33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.59 J/cm²
7.57 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0
Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin..