Polymer Property : Charpy Impact, Notched = 8.23 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.73 J/cm²

@Temperature 23.0 °C
8.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.73 J/cm²
8.23 ft-lb/in²
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned)
Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av..