Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Charpy Impact, Notched 1.89 J/cm²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..