Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.59 J/cm² Grade Count:48 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 0.300 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.95 J/cm² Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 1.50 - 999.9 J/cm² @Temperature -40.0 - 100 °C |
7.14 - 4759 ft-lb/in² @Temperature -40.0 - 212 °F |
Average value: 1.50 J/cm² Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |