Polymer Property : Izod Impact, Notched = 0.0300 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.0300 J/cm

@Temperature 23.0 °C
0.0562 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.0300 - 14.1 J/cm
0.0562 - 26.5 ft-lb/in
Average value: 4.68 J/cm Grade Count:54
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.0300 J/cm
0.0562 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D256
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
Izod Impact, Notched 0.0300 J/cm
0.0562 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East)
Valox 7062 is Mineral filled PBT injection molding grade.
Izod Impact, Notched 0.0300 J/cm

@Temperature -30.0 °C
0.0562 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East)
Valox 7062 is Mineral filled PBT injection molding grade.
Izod Impact, Notched 0.0300 J/cm
0.0562 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.