Mechanical Properties Metric English Comments
Izod Impact, Notched 0.1281 J/cm
0.2400 ft-lb/in
ASTM D256
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA
Derived from annually renewable resources, RenewTech™ BioPlastics 7000 sheet is made with Ingeo™ PLA biopolymer as a base, giving you a packaging solution with competitive cost value performance c..
Izod Impact, Notched 0.1281 - 0.230 J/cm
0.2400 - 0.431 ft-lb/in
90 Minute UV Cure + Thermal; ASTM D256
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..