Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.139 J/cm | 0.260 ft-lb/in | ASTM D256 |
Aclo Accucomp PET PET008L |
|||
Izod Impact, Notched | 0.139 - 100 J/cm | 0.260 - 187 ft-lb/in | Average value: 0.629 J/cm Grade Count:16 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |