Polymer Property : Izod Impact, Notched = 0.204 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.204 J/cm
0.382 ft-lb/in
Abatron AboCast 8-10/Abocure 8-10 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 1 lb. (2.2 kg): 45 minutes; cures in 6 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Ap..
Izod Impact, Notched 0.204 J/cm
0.382 ft-lb/in
ASTM D256
Plenco 7500 Phenolic, Granular, Transfer Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..