Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.206 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.206 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.386 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene 120PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
Izod Impact, Notched 0.206 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.386 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene 129PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP, ELECTRICAL APPLIANCES : ELECTRICAL FAN
Izod Impact, Notched 0.206 J/cm
0.386 ft-lb/in
ASTM D256
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Izod Impact, Notched 0.206 J/cm
0.386 ft-lb/in
Zeon Chemicals Zeonex® E48R Cyclo-Olefin Polymer
Copyright © lookpolymers.com All Rights Reserved