Izod Impact, Notched 0.224238 - 5338.47 J/cm

@Temperature -40.0 - -18.0 °C
0.420090 - 10001.1 ft-lb/in

@Temperature -40.0 - -0.400 °F
Average value: 1.67 J/cm Grade Count:24
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..