Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.170 - 0.270 J/cm | 0.318 - 0.506 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |