Mechanical Properties Metric English Comments
Izod Impact, Notched 0.166713 - 0.274586 J/cm

@Temperature -20.0 - 0.000 °C
0.312322 - 0.514412 ft-lb/in

@Temperature -4.00 - 32.0 °F
Average value: 0.216 J/cm Grade Count:2
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..