Izod Impact, Notched 0.159 - 0.215 J/cm
0.298 - 0.403 ft-lb/in
Average value: 0.186 J/cm Grade Count:11
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..