Mechanical Properties Metric English Comments
Izod Impact, Notched 0.411 J/cm
0.770 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334W40L1 Wollastonite Reinforced
Izod Impact, Notched 0.411 J/cm
0.770 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled
Izod Impact, Notched 0.411 J/cm
0.770 ft-lb/in
ASTM D256
Aaron Industries AAROPRENE® CFPP 2020 Calcium Carbonate Filled Polypropylene
AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.