Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.235 J/cm @Thickness 3.17 mm |
0.441 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® FT6120 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and hi.. |
|||
Izod Impact, Notched | 0.235 J/cm @Thickness 3.17 mm |
0.441 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® FT6125 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.441 ft-lb/in | |
Zeon Chemicals Zeonex® 480 Cyclo-Olefin Polymer |
|||
Izod Impact, Notched | 0.235 J/cm | 0.441 ft-lb/in | |
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer |