Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.190 - 0.240 J/cm | 0.356 - 0.450 ft-lb/in | ASTM D256 |
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Izod Impact, Notched | 0.190 - 0.240 J/cm | 0.356 - 0.450 ft-lb/in | ASTM D256 |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |