Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.246 J/cm | 0.461 ft-lb/in | |
Abatron AboCast 8-17/Abocure 8-17 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 123 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.461 ft-lb/in | |
Abatron AboCast 8-19/Abocure 8-19 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.461 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ NJC-8500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |