Mechanical Properties Metric English Comments
Izod Impact, Notched 0.252 J/cm
0.472 ft-lb/in
ASTM D256A
DSM Somos® 7120 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..