Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.256 J/cm | 0.480 ft-lb/in | ASTM D256 |
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b.. |
|||
Izod Impact, Notched | 0.256 J/cm | 0.480 ft-lb/in | ASTM D256 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.256 J/cm | 0.480 ft-lb/in | |
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system .. |