Mechanical Properties Metric English Comments
Izod Impact, Notched 0.264 J/cm
0.495 ft-lb/in
ASTM D256
Plenco 7080 Phenolic, Nodular, Compression Molded
PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de..