Polymer Property : Izod Impact, Notched = 0.594 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.317 J/cm
0.594 ft-lb/in
ASTM D256A
Total PPH 3462 Polypropylene, Extrusion Grade
Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with..