Polymer Property : Izod Impact, Notched = 0.608 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.608 J/cm
1.14 ft-lb/in
ASTM D256
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber
Izod Impact, Notched 0.608 J/cm
1.14 ft-lb/in
ASTM D256
Cheng Yu Plastic A708G3 SAN, 30% Glass Fiber