Izod Impact, Notched 0.416 J/cm
0.780 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 4012 X Platinum Polypropylene
Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase