Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.838 J/cm @Thickness 3.20 mm |
1.57 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 450S High Gloss HIPS Key features: High-gloss Common Uses: Portable CD-case, air conditioner cases.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impac.. |