Polymer Property : Izod Impact, Notched = 0.85424 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.85424 - 0.85424 J/cm

@Temperature -30.0 - -30.0 °C
1.6003 - 1.6003 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.854 J/cm Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..