Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.13 J/cm | 2.12 ft-lb/in | ISO METHOD 180 |
NYCOA 2012 Copolymer Nylon easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 1.13 J/cm @Temperature -30.0 °C |
2.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific) Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating.. |
|||
Izod Impact, Notched | 1.13 J/cm | 2.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.13 J/cm @Thickness 3.17 mm |
2.11 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® HR-1360 HIPS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.13 J/cm @Thickness 3.17 mm |
2.11 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® HR-1360 HIPS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.13 J/cm | 2.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66 LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare. |
|||
Izod Impact, Notched | 1.13 J/cm | 2.11 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML3425 PC, 25% Glass Fiber |
|||
Izod Impact, Notched | 1.13 J/cm | 2.11 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NG1600S Nylon 66, 60% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 1.13 J/cm | 2.12 ft-lb/in | |
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Izod Impact, Notched | 1.13 J/cm @Temperature -40.0 °C |
2.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.13 J/cm | 2.12 ft-lb/in | compression molded; ASTM D256 |
Americas Styrenics STYRON® 487 High Impact Polystyrene Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A.. |