Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.590 - 1.17 J/cm | 1.11 - 2.20 ft-lb/in | Average value: 0.950 J/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.910 - 1.17 J/cm @Thickness 6.35 mm |
1.70 - 2.19 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.320 - 1.17 J/cm | 0.600 - 2.20 ft-lb/in | Average value: 0.830 J/cm Grade Count:20 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |