Mechanical Properties Metric English Comments
Izod Impact, Notched 0.490 - 0.740 J/cm
0.918 - 1.39 ft-lb/in
Average value: 0.644 J/cm Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..
Izod Impact, Notched 0.214 - 0.740 J/cm
0.401 - 1.39 ft-lb/in
Average value: 0.462 J/cm Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..