Mechanical Properties Metric English Comments
Izod Impact, Notched 0.74746 - 0.74746 J/cm

@Temperature -40.0 - -40.0 °C
1.4003 - 1.4003 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.747 J/cm Grade Count:2
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.74746 - 0.74746 J/cm

@Thickness 3.17 - 3.17 mm
1.4003 - 1.4003 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.747 J/cm Grade Count:2
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.74746 - 1.28136 J/cm

@Temperature -40.0 - -40.0 °C
1.4003 - 2.40051 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.85 J/cm Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched 0.74746 - 1.28136 J/cm

@Thickness 3.17 - 3.17 mm
1.4003 - 2.40051 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.85 J/cm Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..