Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.52 J/cm @Temperature -30.0 °C |
2.85 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EX1632T PC Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available .. |
|||
Izod Impact, Notched | 1.52 J/cm | 2.85 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Izod Impact, Notched | 1.52 J/cm | 2.85 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Izod Impact, Notched | 1.52 J/cm | 2.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Izod Impact, Notched | 1.52 J/cm | 2.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |