Polymer Property : Izod Impact, Notched = 10.8 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.78 J/cm
10.8 ft-lb/in
ASTM D256
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET
Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re..