Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS20LW Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology. Material offers good balance of stiffness and impact properties.Key Applica.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.17 mm |
11.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Centrex® 401 AES Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PCD 0810 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | edgewise; ASTM D256 |
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compressio.. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256A |
LyondellBasell Hifaxâ„¢ CA199AC Thermoplastic Olefin Resin Key Features: low melt flow, medium low modulus, paintable thermoplastic olefin resin, excellent balance of properties, high toughness, good paintability, flexibleApplications: automotive air bag do.. |
|||
Izod Impact, Notched | 5.95 J/cm | 11.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.20 mm |
11.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® T 65 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Engineered Plastics EP Alloy 510B PC/ABS Alloy Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Propert.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Engineered Plastics EP Alloy 510G PC/ABS Alloy Black. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Proper.. |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.17 mm |
11.1 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |