Izod Impact, Notched 11.67 J/cm

@Thickness 3.20 mm
21.86 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM HU1010 PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),..