Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ S206 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Izod Impact, Notched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
IDI Composites 44-10 HGM Thermoset Polyester, Molding Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
IDI Composites A-203 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Izod Impact, Notched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
IDI Composites C-105 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
IDI Composites M-106 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 6.29 J/cm | 11.8 ft-lb/in | |
Kuraray SEPTON® PM3 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |