Mechanical Properties Metric English Comments
Izod Impact, Notched 4.50 - 6.4068 J/cm

@Temperature -40.0 - 0.000 °C
8.43 - 12.003 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 3.96 J/cm Grade Count:6
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..