Polymer Property : Izod Impact, Notched = 13.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 13.0 J/cm
24.4 ft-lb/in
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
Izod Impact, Notched 13.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
24.4 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 13.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
24.4 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 13.0 J/cm
24.4 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...