Polymer Property : Izod Impact, Notched = 14.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 14.0 J/cm
26.2 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom..
Copyright © lookpolymers.com All Rights Reserved