Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 - 99.99 J/cm @Temperature -40.0 - 4.00 °C |
0.300 - 187.3 ft-lb/in @Temperature -40.0 - 39.2 °F |
Average value: 0.779 J/cm Grade Count:89 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |