Mechanical Properties Metric English Comments
Izod Impact, Notched 2.47 J/cm

@Temperature -30.0 °C
4.63 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET
Impact modified PBT+PC+PET, Heat aging improved Xenoy