Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.300 - 2.47 J/cm @Temperature -30.0 - -30.0 °C |
0.562 - 4.63 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.817 J/cm Grade Count:7 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |