Polymer Property : Izod Impact, Notched = 2.74 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.74 J/cm
5.13 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Asia Pacific)
Izod Impact, Notched 2.74 J/cm
5.13 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 (Asia Pacific)
LNP VERTON* RVL28 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Easy Molding.
Izod Impact, Notched 2.74 J/cm
5.13 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL CRX1005 PPE+HIPS (Asia Pacific)
PPE+PS Chemical resistance improved
Izod Impact, Notched 2.74 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
5.13 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® X05516 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Izod Impact, Notched 2.74 J/cm
5.13 ft-lb/in
Wet; ASTM D256
Asahi Kasei Leona® 9400S Nylon 66
Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei