Polymer Property : Izod Impact, Notched = 2.92 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.56 J/cm
2.92 ft-lb/in
ISO METHOD 180
NYCOA 567 PA 6
plasticized general purpose molding and extrusion grade used in shoe heels and mono.Information provided by NYCOA, Inc.
Izod Impact, Notched 1.56 J/cm

@Temperature -30.0 °C
2.92 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EX1332T PC
Lexan* EX1332T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and is UV stabilized. It is availab..
Izod Impact, Notched 1.56 J/cm

@Temperature 23.0 °C
2.92 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp DFP22H PC
LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC..
Izod Impact, Notched 1.56 J/cm
2.92 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific)
PPE+PS, 115 oC HDT