Izod Impact, Notched 0.299 - 21.0 J/cm
0.560 - 39.3 ft-lb/in
Average value: 10.9 J/cm Grade Count:4
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..