Polymer Property : Izod Impact, Notched = 25.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.214 - 13.3 J/cm
0.400 - 25.0 ft-lb/in
Average value: 1.28 J/cm Grade Count:84
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..