Polymer Property : Izod Impact, Notched = 3.22 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.72 J/cm

@Temperature 23.0 °C
3.22 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp DFP22 PC
LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
Izod Impact, Notched 1.72 J/cm
3.22 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC
LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.