Polymer Property : Izod Impact, Notched = 3.32 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.77 J/cm
3.32 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
Izod Impact, Notched 1.77 J/cm
3.32 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS
LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives.